dc.contributor.author | Auwal, İsmail A. | |
dc.contributor.author | Erdemi, Hamit | |
dc.contributor.author | Sözeri, Hüseyin | |
dc.contributor.author | Güngüneş, Hakan | |
dc.contributor.author | Baykal, Abdulhadi | |
dc.date.accessioned | 2019-05-13T08:57:09Z | |
dc.date.available | 2019-05-13T08:57:09Z | |
dc.date.issued | 2016 | |
dc.identifier.citation | Auwal, I. A., Erdemi, H., Sözeri, H., Güngüneş, H., Baykal, A. (2016). Magnetic and dielectric properties of Bi3+ substituted SrFe12O19 hexaferrite. Journal of Magnetism and Magnetic Materials, 412, 69-82. | en_US |
dc.identifier.issn | 0304-8853 | |
dc.identifier.uri | https://doi.org/10.1016/j.jmmm.2016.03.066 | |
dc.identifier.uri | https://hdl.handle.net/11491/860 | |
dc.description.abstract | In the present study, SrBixFe12−xO19 (0.0≤x≤1.0) nanomaterials were successfully synthesized by using chemical co-precipitation method. Products were characterized by X-ray diffraction (XRD), Scanning Electron Microscopy (SEM), Vibrating sample magnetometer (VSM), Mössbauer spectroscopy, AC conductivity and dielectric measurements. The crystal structural information studied by X-ray diffraction (XRD) indicated the formation of single phase pure hexagonal structure, while electron-dispersive X-ray spectroscopy (EDX) revealed the stoichiometric ratio among Bi, Sr, Fe elements. The crystallite sizes of the products were in the range of 65–82 nm. VSM analysis showed a tendency in saturation magnetization as Bi2O3 concentration raises, which can be ascribed to preferential site occupied by Bi3+ ions. The frequency-dependent ac conductivity plots exhibited similar trends for all samples. A significant temperature-dependent behavior was only observed at low and medium frequencies. The replacement of non-magnetic Bi3+ ions by Fe3+ ones having magnetic moment of 5 µB decrease the magnetic moment of 4f1 site. The AC conductivity increases with frequency as hopping of the charge carriers increases between Fe2+and Fe3+. The DC conductivity exhibited an improvement with increasing temperature and Bi content, and the highest conductivity was measured as 2.84×10−9 S cm−1 for x=0.8 at 120 °C. The variation of dielectric constant, dielectric loss and tangent loss was observed with the frequency and temperature due to change of electrical conductivity as x changes. | en_US |
dc.language.iso | eng | |
dc.publisher | Elsevier B.V. | en_US |
dc.relation.isversionof | 10.1016/j.jmmm.2016.03.066 | en_US |
dc.rights | info:eu-repo/semantics/closedAccess | en_US |
dc.subject | AC Conductivity | en_US |
dc.subject | Coprecipitation | en_US |
dc.subject | Dielectric Properties | en_US |
dc.subject | Hexaferrite | en_US |
dc.subject | Magnetic Properties | en_US |
dc.title | Magnetic and dielectric properties of Bi3+ substituted SrFe12O19 hexaferrite | en_US |
dc.type | article | en_US |
dc.relation.journal | Journal of Magnetism and Magnetic Materials | en_US |
dc.department | Hitit Üniversitesi, Fen Edebiyat Fakültesi, Fizik Bölümü | en_US |
dc.identifier.volume | 412 | en_US |
dc.identifier.startpage | 69 | en_US |
dc.identifier.endpage | 82 | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |